Cracked Walls, Epoxy Resin, and Polyurethane
Hydrophilic vs. Hydrophobic Injection Urethane:...
Hydrophilic urethane reacts with water. The moisture in the crack triggers the cure, so it can seal a leak that is still moving. Hydrophobic resins repel water. They need a...
Hydrophilic vs. Hydrophobic Injection Urethane:...
Hydrophilic urethane reacts with water. The moisture in the crack triggers the cure, so it can seal a leak that is still moving. Hydrophobic resins repel water. They need a...
Crack Injection or Surface Seal? Choosing the Fix
Crack injection puts material inside the crack through ports and fills the void. It's a repair. It restores the wall's continuity across the crack and stops water from passing through...
Crack Injection or Surface Seal? Choosing the Fix
Crack injection puts material inside the crack through ports and fills the void. It's a repair. It restores the wall's continuity across the crack and stops water from passing through...
Matching Viscosity to Crack Width: Which Inject...
Viscosity is the one variable you choose before you climb the ladder. Here's how to match it to the crack in front of you.
Matching Viscosity to Crack Width: Which Inject...
Viscosity is the one variable you choose before you climb the ladder. Here's how to match it to the crack in front of you.